Never seen that before so I would'nt know how good it worked. I would use Artic Silver Ceramique for phase cooling.
 
the day i go -0 is getting closer... but its not here yet sorry

(i have checked out where the closest Ln2 supplier is though)



WTB JoeC's diamond stuff =p

OK


-LINK-


:beer:

the stuff is CRAZY tough to apply ... its like ummm.... sandy clay ... barley moist


how i apply it is:

5x "large BB" sized dots on IHS (center and "close" to the 4 corners)
pressure spread (mount HSF)
un-mount
apply BB's to fill in gaps
pressure spread again
un-mount again
(repeat as necessary)
wait the 10 min for solvent to evaporate
and then final mount.


gets a little tricky because 1/3 of the stuff always seems to pull off and stick to the HSF while the other 2/3 stays on the IHS :-/
 